In the pulp preparation workshop of a ceramics factory, the most frequently adjusted additive is probably the water-reducing agent. Even a small amount can simultaneously affect the slurry's fluidity, water content, ball milling efficiency, green body strength, and the fuel costs of spray drying. Many on-site problems—such as slurry settling and stratifying in the storage tank, low output from the spray tower, and cracking of bricks during drying—can ultimately be traced back to the debinding process.
Clay minerals (kaolin, bentonite, illite, etc.) in ceramic blanks dissociate into charged surfaces in water. These particle surfaces are typically negatively charged, but naturally occurring high-valence cations such as Ca²⁺, Mg²⁺, and Fe³⁺ in the clay are adsorbed onto the particle surfaces, neutralizing some of the charge and weakening the electrostatic repulsion between particles. With this weakened repulsion, the particles move closer together and clump together using van der Waals forces, trapping a large amount of free water inside the clumps.
The macroscopic manifestation is that the mud appears to have a lot of water, but its fluidity is poor, its viscosity is high, and its water content cannot be reduced. The idea of adding a degelatinizing agent is very straightforward—introduce monovalent cations such as Na⁺ to replace the high-valent cations from the particle surface, allowing the double layer to thicken again, the particles to redisperse, and the locked water to be released.
One sentence to understand
Deflocculation doesn't reduce the amount of water; rather, it releases the water that was previously trapped within the flocs . Therefore, at the same fluidity, the water content of the slurry can be significantly reduced, thus decreasing the evaporation load of the spray dryer.
Even though they are all water-reducing agents, solid powders, liquids, composite trimers, and sodium metasilicate behave differently in clay systems. Before selecting a type, it's essential to identify the type of clay you are dealing with.
Table 1 Comparison of Basic Inorganic Salt Degumming Products
| Product Form | Appearance and Packaging | Typical ingredients | More suitable clay |
|---|---|---|---|
| Solid ceramic water-reducing agent | White powder, maximum particle size 3mm, packaged in an inner woven bag weighing 25kg/bag. | Na₂O、SiO₂、Fe₂O₃、K₂O、MgO、TiO₂ | It is suitable for both mud making and pulp grinding, including for lean raw materials; it is convenient for feeding and metering. |
| Liquid degumming agent | Colorless or pale yellow liquid, 25kg/drum PVC plastic container. | Na₂O、SiO₂、Fe₂O₃、P₂O₅、K₂O、MgO、TiO₂ | Bentonite with low water content; slurry and glaze with high aluminum, calcium, magnesium and iron content. |
| Complex trimer | White powder, maximum particle size 2mm, 25kg/bag | Na₂O、SiO₂、Fe₂O₃、P₂O₅ | Slurries and glazes with high aluminum, calcium, and magnesium content have a wide degelatination range. |
| Sodium metasilicate pentahydrate | White powder, maximum particle size 3mm, 25kg/bag | Na₂O、SiO₂、Fe₂O₃、K₂O、MgO、TiO₂ | Strongly alkaline system; combines detergency, buffering, and metal corrosion protection. |
Note: The table above shows standard specifications. Solid content, viscosity, particle size, and other indicators can be adjusted according to customer requirements. For organic polymer routes (such as ceramic body reinforcing agents and glaze dispersants), please refer to the corresponding articles.
The company's product information states that the commonly used range is 0.1% to 0.5% of the dry powder weight . This range is wide because the composition of clay minerals varies greatly: clay with high bentonite content has a larger surface area and more surface charge, requiring more degumming agent; while raw materials mainly composed of kaolin often only require less than 0.2%.
Many factories treat defatting agents as a quick fix for poor flowability, adding them to the slurry storage tank. While this does improve flowability, it misses the most valuable window of opportunity—the ball milling stage.
Adding the desiccant before ball milling allows its lubricating and grinding-aiding effects between particles to be fully realized: ball milling time is shortened, unit power consumption is reduced, and the water content of the slurry is lowered from the source. Adding it after grinding only saves on stirring resistance.
Both feeding methods are feasible: dissolve in water first and then mix with raw materials, or add directly to dry materials, mix well, and then slurry. Liquid deflocculants are more convenient in this respect, as they can be directly metered and pumped, making them particularly suitable for automated batching lines.
More adhesive release agent is not necessarily better. If the following phenomena occur on-site, first suspect that the dosage is too high, rather than continuing to add more:
If possible, add water-reducing agent according to the actual formula in a small ball mill jar, grind, and then measure the slurry's moisture content and fluidity. Then press it into small bricks to compare their flexural strength—this is consistent with the testing method recommended in the company's product documentation. Measuring only fluidity without considering strength can easily lead to the erroneous judgment of "good flow, brittle blank."
In addition, this type of product is non-toxic, non-polluting, and non-radioactive. After use, it should be sealed and stored in a dry, cool place. Storage conditions should be planned before large-scale production to prevent moisture and clumping from affecting measurement accuracy.
打开微信分享“扫一扫”
即可分享到微信分享

Long by picture save/share

Email: JEFF@CSCHEMICA.NET
Headquarters Address: Room 1806-1808, Building 36, Yiyun Xicheng, Keji North Road, Shishan Town, Nanhai District, Foshan City
Factory Address: Datianfeng Industrial Zone, Wuzhuang, Luocun, Shishan Town, Nanhai District, Foshan City

© 2026 Foshan Chaoso Technology Co., Ltd. All Rights Reserved Yue ICP Bei No. 2020092827-1 Technical Support:Sheyu Technology